You can see where around corners and even some straight runs it is peeling up. I'm running first layer at an agonizing 15 mm/s. Using hatchbox pla filament, just dried in dehydrator. 200° nozzle and 70° bed. The glass is freshly cleaned with soap and water, I just did several atomic pulls, I've trammed at different heights using a feeler gauge, and absolutely nothing is working. Any one have any ideas?

you are viewing a single comment's thread
view the rest of the comments
[–] Keesrif 2 points 10 months ago

On top of some of the other tips, layer height being the most prominent, perhaps try a different soap or clean it with alcohol after. I've noticed a difference between soaps (and even between toilet paper brands) - some things leave a bit of residu I think.