You can see where around corners and even some straight runs it is peeling up. I'm running first layer at an agonizing 15 mm/s. Using hatchbox pla filament, just dried in dehydrator. 200° nozzle and 70° bed. The glass is freshly cleaned with soap and water, I just did several atomic pulls, I've trammed at different heights using a feeler gauge, and absolutely nothing is working. Any one have any ideas?

you are viewing a single comment's thread
view the rest of the comments
[–] 20inmyhead@lemmy.ml 2 points 10 months ago (1 children)

+1 for upping the temp. I always find printing the first couple layers at 5° hotter to helps a lot with adhesion.

[–] BingoBangoBongo@midwest.social 2 points 10 months ago

Increase in temp seemed to help!